Skip to main content
. Author manuscript; available in PMC: 2018 Oct 30.
Published in final edited form as: Soft Matter. 2017 Aug 30;13(34):5684–5695. doi: 10.1039/c7sm00727b

Table II.

Composition of the pS-co-NIPAM series and a comparative size analysis using SEM and AFM.

Microgel Sample Composition (mol%) (Styrene:NIPAM: BIS) Diameter (nm)
(Dried, SEM)
Height (nm)
(Dried, AFM)
Width (nm)
(Dried, AFM)
Aspect ratio
(Width/Height, AFM)
pS-co-NIPAM-1 50:50:0 170 ± 5 200 ± 4 247 ± 12 1.23 ± 0.06
pS-co-NIPAM-2 49.5:49.5:1 175 ± 4 213 ± 4 247 ± 6 1.16 ± 0.04
pS-co-NIPAM-3 48.5:48.5:3 164 ± 4 187 ± 2 238 ± 8 1.27 ± 0.04
pS-co-NIPAM-4 24.75:74.25:1 171 ± 8 181 ± 5 254 ± 10 1.40 ± 0.07
pS-co-NIPAM-5 24:73:3 190 ± 6 170 ± 7 252 ± 10 1.48 ± 0.08