Table 2.
Thickness (μm) | Mass (g) | Width (cm) | Length (cm) | Volume (cm3) | Density (g/cm3) |
---|---|---|---|---|---|
200 | 2.50 | 0.965 | 2.29 | 1.67 | 0.98 |
100 | 0.79 | 0.940 | 2.34 | 1.62 | 0.48 |
500 | 0.77 | 0.050 | 2.25 | 0.12 | 0.50 |
HR (°C/min) | SARExp (W/cm3) | Metal type and structure | SARExp (W/g) | SARExp/SARThe (%) | |
---|---|---|---|---|---|
1200 | 80 | Copper foam | 82 | 80 | |
1000 | 200 | Aluminum foil | 415 | 92 | |
330 | 480 | Nitinol mesh | 960 | 96 |
Heating rates and experimental SARs are calculated from the linear portion of the heating profile