Physical properties of copper foam, aluminum foil and nitinol mesh.

Thickness (μm) Mass (g) Width (cm) Length (cm) Volume (cm3) Density (g/cm3)
200 2.50 0.965 2.29 1.67 0.98
100 0.79 0.940 2.34 1.62 0.48
500 0.77 0.050 2.25 0.12 0.50
HR (°C/min) SARExp (W/cm3) Metal type and structure SARExp (W/g) SARExp/SARThe (%)
1200 80 Copper foam graphic file with name 10439_2018_2063_Figa_HTML.gif 82 80
1000 200 Aluminum foil graphic file with name 10439_2018_2063_Figb_HTML.gif 415 92
330 480 Nitinol mesh graphic file with name 10439_2018_2063_Figc_HTML.gif 960 96

Heating rates and experimental SARs are calculated from the linear portion of the heating profile