Skip to main content
. 2018 Nov 2;8:16282. doi: 10.1038/s41598-018-34644-9

Figure 6.

Figure 6

Migration of small graphene flakes during pyrolysis. (A–C) Separation of a circular flake from a larger graphene mass (arrow 1). (D-F) merger of a flake (which was absent from the field of view at 640 °C) into a neighbouring material at 780 °C (arrow 2). All scale bars: 2 nm.