Skip to main content
. 2018 Sep 20;8(10):747. doi: 10.3390/nano8100747

Table 2.

Summary of the asymmetric SCs based on NiMn LDH and carbon electrodes.

Negative Electrode Positive Electrode Power Density (kW kg−1) Energy Density (Wh kg−1) Potential (V) References
rGO Flower-like NiMn LDH/rGO 0.4 29.3 1.6 [37]
rGO NiMn-LDH/rGO 1 22.5 1.8 [49]
AC NiMn-LDH/rGO 0.85 33.8 1.7 [24]
rGO/CNT NiMn LDH/CNTs 0.85 88.3 1.7 [48]
AC Polyhedral NiMn LDH@carbon 0.225 18.6 1.5 [51]
rGO NiMn-LDH/rGO 1.68 74.7 1.6 [28]
AC NiO/NiMn LDH@Ni foam 0.41 27.8 1.6 [53]
AC Carbon coated NiMn LDH @Ni foam 0.378 37.7 1.5 [36]
Graphene KCu7S4/NiMn LDHs@Ni foam 0.65 15.9 1.5 [30]
AC CuCo2S4/NiMn LDH@Ni foam 1.499 45.8 1.5 [57]
AC Ni3S2/NiMn LDH@Ni foam 0.6 68 1.6 [56]
AC LDH/vertical graphene@Ni foam 0.26 56.8 1.6 [55]
AC NiCoMn LDH/rGO 4.24 42.4 1.8 [61]
rGO NiCoMn-(LDH) (10% Co) 0.75 57.4 1.5 [39]