Skip to main content
. 2018 Sep 30;23(10):2515. doi: 10.3390/molecules23102515

Figure 7.

Figure 7

Results of self-healing at 130 °C for 120 min: (a) tensile properties of H-PU after self-healing; (b) tensile properties of S-PU after self-healing; (c) schematic of the self-healing mechanism and configurational change of typical S-PU after the exchange reaction.