Table 1.

Impedance parameters of ZnCo2O4–Li after different cycles in the fully charged state

Fresh cell 10th-charge cycle 50th-charge cycle 70th-charge cycle 100th-charge cycle
OCV (V vs. Li) open-circuit voltage 2.2 2.85 2.90 2.80 2.90
R e (Ω) electrolyte resistance 3.9 4.4 4.0 4.2 4.1
R (sf+ct) (Ω) surface film + charge transfer resistance 149.4 72.8 47.1 47.9 48.2
CPE(sf+dl) (µF) constant phase element due to surface film + double layer capacitance 12 160 125 113 102
W s (Ω) Warburg resistance 690 2969 3826 3838 3894
C i (µF) intercalation capacitance 284 4.7 3.5 3.0 2.8