a Average thickness of tailored PVP nanolayer before and after further washing treatment in DMF or DI water.Inset: morphology of tailored PVP nanolayer after further dissolution treatment. Scale bar = 5 nm. b Sheet resistance of AgNW electrodes with high transmittance above 95 % at 550 nm wavelength, employing E4-AgNWs and AgNWs further treated in DMF or DI water