Skip to main content
. 2018 Oct 4;122(43):24917–24923. doi: 10.1021/acs.jpcc.8b07283

Figure 4.

Figure 4

Emission lifetime traces of tetra-tert-butylperylene-loaded cavities (a–c) measured at different angles between 10 and 60° and the internal machine response (black). The decays show no change of fitted lifetime within the same cavity when varying the detection angle.