Skip to main content
. 2018 Oct 18;57(44):15147–15158. doi: 10.1021/acs.iecr.8b03723

Figure 1.

Figure 1

Effect of the L:W ratio on the removal of eucalyptus wood chip components and on the intrinsic viscosity of the pulp. The fractionation trials were conducted in 50 wt % GVL solution, at 180 °C, for 150 min, and with varying L:W ratios, from 2 L/kg to 10 L/kg in the air-bath digester. [Note: the abbreviation odw represents oven-dried wood.]