Figure 3.

Figure 3

Optical characterization of the NaYF4 NPs. (a) OTN-NIR emission spectra of NaYF4 NPs obtained at 25, 37, and 46 °C under 980-nm excitation. (b) Normalized PL intensity of Ho3+ and Er3+. (c) Calibration curve of the NaYF4 NPs of the relationship between IHo/IEr ratio and temperature. (d) Relative thermal sensitivity and (e) temperature uncertainty as functions of temperature for the NaYF4 NPs. The NPs were dispersed in cyclohexane at a concentration of 11 mg/mL. The laser power was 4.22 W.