Skip to main content
. 2018 Nov 21;8:17213. doi: 10.1038/s41598-018-35632-9

Table 1.

Physicochemical and mechanical evaluations of hydrophobically modified alginate-psyllium husk gel composite film.

Concentration (in % w/v) Thickness (in mm) study in triplicate Weight variation (in g) study in triplicate Folding endurance (no. of times) % Elongation study in triplicate % Swelling study in triplicate In vitro deformation (in min) study in triplicate
4% Psyllium gel 1.40 ± 0.1 0.035 ± 0.002 128 ± 0.01 6.32 ± 0.03 NA NA
4.75 (4% Psyllium gel + 0.75% alginate) 0.35 ± 0.02 0.472 ± 0.01 135.33 ± 0.57 24.28 ± 0.02 14.30 ± 0.02 5.5 ± 0.01
5 (4% Psyllium gel + 0.75% alginate + 0.25% lauryl grafted alginate) 0.37 ± 0.02 0.481 ± 0.001 137 ± 0.01 27.28 ± 0.02 15.39 ± 0.03 5.9 ± 0.05