Skip to main content
. 2018 Nov 23;4:8–16. doi: 10.1016/j.bioactmat.2018.11.001

Fig. 7.

Fig. 7

SEM fracture surface for tensile specimens of (a) the as-cast Zn-0.4 Mg alloy, the (b) as-rolled pure Zn, (c) as-rolled Zn-0.4 Mg alloy, and (d) as-rolled Zn-0.8 Mg alloy.