Content of each functional group of graphite oxide prepared at different reaction temperatures.

Sample Relative Percentage Content /% C/O
C=C C−OH Epoxy Groups O−C=O
GO-0 53.75 23.08 18.03 5.14 2.09
GO-30 43.80 28.77 19.95 7.48 1.90
GO-50 42.58 30.01 19.72 7.69 1.85
GO-60 42.23 27.92 21.33 8.52 1.86
GO-70 44.78 25.27 21.40 8.54 1.89
GO-80 45.42 21.33 22.93 10.31 2.06
GO-100 45.83 20.18 22.96 11.03 2.23