. 2018 Nov 3;18(11):3759. doi: 10.3390/s18113759

Figure 2.

Figure 2

XRD patterns of the [90–10] MoSi2-Al2O3, WSi2-Al2O3, TaSi2-Al2O3, and ZrSi2-Al2O3 composites after sintering at 1500 °C for 2 h.