Skip to main content
. 2018 Nov 3;18(11):3759. doi: 10.3390/s18113759

Figure 3.

Figure 3

SEM micrographs of the [90–10] (a) MoSi2-Al2O3, (b) WSi2-Al2O3, (c) TaSi2-Al2O3, and (d) ZrSi2-Al2O3 composites after sintering at 1500 °C for 2 h.