Figure 11.

Figure 11

Figure 11

Micrographs of Mg-13.5Gd-3.2Y-2.3Zn-0.5Zr alloy compressed at 400 °C, 440 °C and 480 °C at the strain rate of 0.001/s, 0.01/s, 0.1/s and 1/s.