Skip to main content
. 2018 Nov 12;11(11):2249. doi: 10.3390/ma11112249

Table 2.

Material properties of poly(urethane acrylate) aerogels with aromatic core before (aR-PUAc-xx) and after (aR-PUAc-xx-C) 1 pyrolysis.

Sample Skeletal Density ρs (g cm−3) BET Surf. Area σ (m2 g−1) [Micropore Surf. Area] 2 Quantity of CO2 Adsorbed (mmoL g−1)
aR-PUAc-1.5 1.40 ± 0.01 488 [38] 0.63
aR-PUAc-1.5-C 2.0 ± 0.1 171 [154] 1.09
aR-PUAc-6 1.454 ± 0.004 374 [18] 0.97
aR-PUAc-6-C 2.15 ± 0.03 639 [360] 2.50
aR-PUAc-12 1.414 ± 0.006 311 [2] 0.84
aR-PUAc-12-C 2.3 ± 0.1 739 [429] 0.99

1 Pyrolyzed at 800 °C for 5 h under flowing Ar. 2 Micropore surface area via t-plot analysis, according to the Harkins and Jura model.