Skip to main content
. 2018 Nov 1;11(11):2153. doi: 10.3390/ma11112153

Table 4.

Development of compressive strength and short-term water absorption of bio-composite with binder composition of B7 in relation to hardening time.

Hardening Time (Days) Short-Term Water Absorption (%) Compressive Strength (MPa)
28 15.3 ± 0.74 3.51 ± 0.17
60 11.1 ± 0.53 4.59 ± 0.28
90 8.9 ± 0.41 8.12 ± 0.62