(a) Mott–Schottky plots of treated-TiO2 and TiO2 at 5 kHz in 1 mol·dm−3 AlCl3/1 mol·dm−3 KCl; (b) Mott–Schottky plots of the treated TiO2 electrode at 2, 5 and 10 kHz.