Sample Impact Strength (kJ·m−2) Shore D Hardness
PLA 2.14 ± 0.28 73.1 ± 1.3
PLA60PCL40TPS0 6.52 ± 0.62 63.0 ± 1.0
PLA60PCL30TPS10 6.46 ± 0.39 63.6 ± 1.1
PLA60PCL20TPS20 6.51 ± 0.27 63.7 ± 1.2
PLA60PCL10TPS30 6.33 ± 0.24 64.3 ± 1.1
PLA60PCL0TPS40 5.46 ± 0.88 64.6 ± 1.1