Skip to main content
. 2018 Nov 9;8(11):933. doi: 10.3390/nano8110933

Figure 5.

Figure 5

Contact angle of the SiNPs/PVDF nanocomposites: (a) PVDF with the SiNPs with different diameters processed at 90 °C and (b) SiNPs/PVDF samples with silica nanoparticles (17 nm) with different morphologies.