Skip to main content
. 2018 Nov 1;11(11):2152. doi: 10.3390/ma11112152

Figure 11.

Figure 11

Variation of transepidermal water loss (TEWL) and skin capacitance (hydration) between initial and 24 h of skin application of cotton and polyamide fabrics. NT: non-treated fabric. Internal wool lipids (IWL): fabric treated with IWL liposomes. PC: fabric treated with PC liposomes (* p < 0.05 corresponds to significant difference between the marked columns).