Figure 8.

Figure 8

The development of the infrared absorption characteristic of carbonyl oxidation products in an unpigmented polyethylene film as the UV exposure in QUV accelerated weathering equipment, fitted with UVA-340 tubes and operated at 40 °C, increases from 125 to 1348 h. (reprinted from Polymer Degradation and Stability. 2007, 92, 2163–2172 [41] with permission).