Skip to main content
. 2014 Apr 24;19(4):5348–5359. doi: 10.3390/molecules19045348

Figure 3.

Figure 3

Polarized light photomicrographs for the PS/PO oil blends under 120 MPa HPM treatment: (a) Treated once and crystallized 0 h, 4 h, 1 day and 5 days. (b) Treated twice and crystallized 0 h, 4 h, 1 day and 5 days respectively. Magnification 500×.