Table 3.
Treatments | ||||
---|---|---|---|---|
Fiber Type | Sample Size | Temperature | Time | Sample Agitation |
85 µm CPDMS | 0.25 mL | 25 °C | 1 h | None |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
0.25 mL | 37 °C | 1 h | None | |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
75 µm CPDMS | 0.25 mL | 25 °C | 1 h | None |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
0.25 mL | 37 °C | 1 h | None | |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
50/30 µm DVB/CPDMS | 0.25 mL | 25 °C | 1 h | None |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
0.25 mL | 37 °C | 1 hour | None | |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
100 µm PDMS | 0.25 mL | 25 °C | 1 h | None |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
0.25 mL | 37 °C | 1 h | None | |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
65 µm PDMS/DVB | 0.25 mL | 25 °C | 1 h | None |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm | ||
0.25 mL | 37 °C | 1 h | None | |
0.50 mL | 24 h | 0.20 cm × 0.50 cm Stir bar @ 1000 rpm |
Abbreviations: CAR/PDMS = Carboxen polydimethylsiloxane; DVB/CAR/PDMS = divinylbenzene/ Carboxen polydimethylsiloxane; PDMS = polydimethylsiloxane; PDMS/DVB = polydimethyl-siloxane/divinylbenzene.