Skip to main content
. Author manuscript; available in PMC: 2018 Dec 3.
Published in final edited form as: J Appl Polym Sci. 2012 Aug 1;128(3):1804–1814. doi: 10.1002/APP.38335

Figure 10.

Figure 10.

Batch dechlorination of TCE with Fe/Pd (Pd = 1.5 wt %) (70 nm) immobilized in P(NIPAAm-AA) hydrogel at 30°C (below LCST) and 34°C (above LCST). Vol. = 43 mL, pH = 6.8; initial TCE concentration: 30 mg L−1, iron loading amount: 0.3 g L−1. [Color figure can be viewed in the online issue, which is available at wileyonlinelibrary.com.]