Table 4.

Langmuir and Freundlich parameters and compared maximum adsorption capacity of BPA and diuron on ANS@H2O-120 with different adsorbents

Langmuir Freundlich
Q max
(mg/g)
K L
(L/mg)
R L R 2 K F
(mg/g)/(mg/L)n
n R 2
BPA 1408 24.483 0.001 0.9576 1569 0.757 0.6192
Diuron 1087 5.412 0.005 0.9646 1166 1.343 0.6228
Microporous carbon Specific surface area (m2/g) Adsorption capacity (mg/g) Reference
Bisphenol A
ANS@H2O-120 2853 1408 Current study
Activated carbon (AC-HP) 1372 1250 (Zbair et al. 2018b)
Activated carbon (Takeda) 1119 23.5 (Nakanishi et al. 2002)
Graphene 327 181.6 (Xu et al. 2012)
mesoporous carbon (CMK3) 920 296 (Sui et al. 2011)
Activated carbon 1760 432.3 (Liu et al. 2009)
Activated carbon powder 771.2 (Li et al. 2014)
CoFe2O4/activated carbon 727.2 (Li et al. 2014)
Diuron
ANS@H2O-120 2853 1087 Current study
Activated carbon 2128 292.9 (López-Ramón et al. 2007)
Activated carbon fiber 1709 667.2 (López-Ramón et al. 2007)
Activated carbon 776 279.4 (Ángeles Fontecha-Cámara et al. 2006)
Activated carbon 1139 51.2 (Bahri et al. 2012)
Carbon nanotubes 258.6 39.6 (Sun et al. 2012)