Thermoelectric properties of the p-type CNT samples at room temperature.

Materials Electrical Conductivity
[S/cm]
Seebeck Coefficient
[μV/K]
Power Factor
[μW/m K2]
Ref.
DWNT-CSA ~1.7 × 104 ~18 550.80 [70]
DWNT-NMP ~1500 ~55 453.75 [70]
DWNT-SDBS ~2400 ~36 311.04 [70]
ASWNT-CSA ~3100 ~28 243.04 [70]
ASWNT-NMP ~500 ~40 80 [70]
ASWNT-SDBS ~700 ~24 40.32 [70]