Skip to main content
. 2018 Oct 26;10(11):1196. doi: 10.3390/polym10111196

Table 2.

Thermoelectric properties of the n-type CNT samples at room temperature.

Materials Electrical Conductivity
[S cm−1]
Seebeck Coefficient
[μV K−1]
Power Factor
[μW m−1 K−2]
Ref.
SW-PEI 10 −58 3.4 [75]
DWNT-PEI/graphene-PVP 297 −80 190 [76]
SWCNT-PDINE 500 −47.3 112 ± 8 [81]
SWCNT-NDINE 446 −55 135 ± 14 [81]