Table 1.
Filler | Matrix | κ (W/mK) | Fraction | Years |
---|---|---|---|---|
Graphite nanoplatelet | Epoxy | 6.44 | ≈34 wt % | 2007 [14] |
Functionalized exfoliated graphite | Epoxy | 5.80 | 20 wt % | 2008 [15] |
Graphene + CNT | Epoxy | 0.32 | 1 wt % | 2011 [16] |
Graphene + Multilayer graphene | Epoxy | 5.10 | ≈15 wt % | 2012 [7] |
Graphene + CNT | Epoxy | 7.30 | 50 wt % | 2012 [17] |
Functionalized graphene flakes | Epoxy | 1.53 | 10 wt % | 2013 [18] |
Graphene nanoflake | Polytetrafluoroethylene | 10.00 | ≈24 wt % | 2015 [19] |
Graphene nanoplatelets | Polycarbonate | 7.30 | 20 wt % | 2016 [20] |
Multilayer graphene | Epoxy | 1.50 | 5.7 wt % | 2016 [11] |