Table 1.

Fe3O4 NPs-Biocorona Characterization.

Nanoparticle - BC Hydrodynamic size
(nm)
Polydispersity
index
Zeta potential (mV)
Fe3O4-H2O 143.0 ± 2.4 0.26 ± 0.01 −41.13 ± 1.31
Fe3O4-SFM 76.1 ± 1.9* 0.15 ± 0.01* −37.77 ± 0.85
Fe3O4-FBS 332.0 ± 9.3*,# 0.28 ± 0.02# −34.53 ± 0.26*
Fe3O4-FBS + LDL 525.6 ± 18.5*,#,+ 0.40 ± 0.02# −20.28 ± 1.05*,#,+

Note: Data represent mean ± SEM, n = 9–12/group.

*

p < 0.05, as compared with the Fe3O4-H2O.

#

p < 0.05, as compared with the Fe3O4-SFM.

+

p < 0.05, as compared with the Fe3O4-FBS.