Skip to main content
. Author manuscript; available in PMC: 2019 Dec 1.
Published in final edited form as: Biomaterials. 2018 Sep 18;185:194–204. doi: 10.1016/j.biomaterials.2018.09.027

Figure 9.

Figure 9.

Effect of scaffold chemistry (PFDMA vs PLA films) and scaffold porosity (PFDMA polyHIPE vs PFDMA film) on calcium deposition in cell free conditions (A). Quantification of hMSC adhesion on varied substrate determined by dsDNA quantification (B). Effect of substrate on hMSC alkaline phosphatase activity after 14 days (C). Cells were cultured in growth media (GM) and osteogenic media (OM) as positive control. All data represents average ± standard deviation for n = 4. The * represents significant difference (p<0.05) for indicated composition compared to all others in respective media.