Figure 2.

Figure 2

a) SEM images of samples 1–4, showing AgNWs embedded in parylene films with different densities. b) Transmittance spectra of samples 1–4 in the wavelength range from 350 to 1200 nm, using a 3 µm thick parylene film as the reference group. c) The relationship between sheet resistance and transmittance at 550 nm of samples 1–4. d) Changes in sheet resistance of samples 1–4 exposed in air at room temperature. e) Variations in normalized sheet resistance of the hybrid film during bending test. The inset shows the experimental setup.