Table 5.
Electrolyte composition and obtained dc conductivity values for LiClO4 incorporated solid polymer electrolytes.
| S.No | Electrolyte composition | dc conductivity at RT (S cm−1) | References |
|---|---|---|---|
| 1. | Thermoplastic Polyurethane-LiClO4 | 8.89 × 10−5 | [61] |
| 2. | Poly ethylene oxide-Poly methyl methacrylate- LiClO4 | ∼10–5 | [62] |
| 3. | Poly vinyl chloride- Poly methyl methacrylate - LiClO4 | 7.17 × 10−3 | [63] |
| 4. | Poly ethylene oxide –Poly vinyl pyrrolidone - LiClO4 | 2.3 × 10−6 | [59] |
| 5. | Gelatin- LiClO4 | 1.04 × 10−4 | [64] |
| 6. | Poly ethyl methacrylate – LiClO4 | 2.34 × 10−6 | [56] |
| 7. | Poly ethylene oxide – LiClO4 | ∼10–6 | [57] |
| 8. | Poly vinyl pyrrolidone – LiClO4 | ∼5 × 10−5 | [58] |
| 9. | Poly vinyl acetate/Poly methyl methacrylate – LiClO4 | 1.76 × 10−3 | [60] |
| 10. | Poly vinyl pyrrolidone - LiClO4 | IR only | [65] |
| 11. | Poly vinylidene fluoride- LiClO4 | ∼10–5 | [66] |
| 12. | Poly(bis(pentyl amino phosphazene) - LiClO4 | 8.1 × 10−3 | [67] |
| 13. | Poly ethylene oxide -PES- LiClO4 | 3 × 10−5 | [68] |
| 14. | Poly propylene oxide-LiClO4 | ∼10−5 at 70 °C | [69] |
| 15. | Poly ethylene oxide -LiClO4-α alumina | 5.2 × 10−4 | [70] |
| 16. | Poly ethylene oxide - PVDF-HFP-LiClO4-TiO2 | 2.27 × 10−4 | [71] |
| 17. | Poly ethylene oxide - PVDF-HFP-LiClO4-SrTiO3 | 4.82 × 10−5 | [72] |
| 18. | Poly ethylene oxide - LiClO4-SiO2 | 2.3 × 10−5 | [73] |
| 19. | Poly vinyl chloride - LiClO4 – ZnO | 3.7× 10−7 | [74] |