Skip to main content
. 2018 Dec 8;4(12):e00992. doi: 10.1016/j.heliyon.2018.e00992

Table 6.

Electrolyte composition and dc conductivity values for plasticized polymer electrolytes which contain LiClO4 as ionic salt.

S.No Electrolyte composition dc conductivity at RT (S cm−1) References
1. P(VdF-co-HFP):PVAc – LiClO4 [78]
2. P(VDF-co-HFP)/PMMA- LiClO4 [79]
3. poly(vinyl sulfone) – and poly(vinylidene fluoride) – LiClO4/LiN(CF3SO2)2/LiAsF6 10−4 to 10−3 [80]
4. PEO – PVP – LiClO4 – EC 2.72× 10−4 [81]
5. PAN – LiClO4 – EC IR only [82]
6. PAN – PC – 1,4-butyrolactone – DMSO – LiClO4 4.7 × 10−3 [83]
7. PEO – P(VDF-co-HFP) – LiClO4 – PC 2.39 × 10−3 [63]
8. PVDF – LiClO4 – PC ∼10–5 [66]
9. Chitosan – Starch – Glyscerol – LiClO4 3.7 × 10−4 [84]
10. PEO – LiClO4 – DOP-νAl2O3 4.29 × 10−4 [85]
11. PMMA – LiClO4 – DMP-CeO2 5.36 × 10−5 [86]
12. PMMA – LiClO4 – PC-SiO2 ∼10–3 [87]
13. P(VDFcoHFP) – PVAc – LiClO4 – EC-PC 2.3 × 10−3 [78]
14. PVDFcoHFP – PMMA – LiClO4 – PC ∼10−3 [79]
15. PVP – LiClO4 – PC-BaTiO3 1.2× 10−3 [88]
16. PVS – PVDF – LiClO4 – EC-PC-Sulfolane ∼10−3 [80]
17. PAN – LiClO4-ED4CN-PC 1.05 × 10−2 [89]
18. PPC – LiClO4 – BMIMBF4 1.5 × 10−3 [90]
19. PEO – LiClO4 – d2000 1.5 × 10−5 [91]
20. PVDF – PVC – LiClO4 – EC – PC 4.68 × 10−3 [92]
21. PVC – PAN – LiClO4 – EC – TiO2 4.46 × 10−3 [93]
22. P(VDF-co-HFP) – PVDF – LiClO4 – PC – DEC 7.5 × 10−3 [94]