Skip to main content
. 2018 Dec 6;8(12):1016. doi: 10.3390/nano8121016

Figure 1.

Figure 1

Particle size, size distribution, and LC loading capacities of PLA nanoparticles prepared under different PVA concentrations (water–oil ratio was 4:3, PLA concentration was 133 g/L, and LC-PLA ratio was 1:1).