Skip to main content
. 2018 Dec 6;8(12):1016. doi: 10.3390/nano8121016

Figure 6.

Figure 6

Particle size, size distributions, and LC loading capacities of PLA nanoparticles prepared under different LC-PLA ratios (PVA concentration was 2%, water–oil ratio was 4:3, PLA concentration was 133 g/L, and the amount of LC was constant).