Table 1.
Materials | Bonding Method | Bonding Time (h) |
Maximum Bonding Strength (MPa) |
Test Method |
---|---|---|---|---|
PDMS–Glass [31] | Plasma | 0.5~2 | 0.51 | Pressure injection |
PDMS–PDMS [36] | Plasma | 0.5~2 | 0.55 | Pressure injection |
Glass–Glass [37] | Microwave oven | 1 | >1 (assume: 1 to 30) | Pressure injection |
Glass–Glass [38] | Anodic | 24 | 29.7 | Tensile test |
Glass–Glass [39] | Pyrex | 1.3 | 2.5 | Tensile test |
Glass–Glass | UV adhesive | 0.5 | 1.1 | Pressure injection |
Glass–Glass | Laser welding (this work) |
<0.08 (5 min) |
>1.4 | Pressure injection |
7.5 | Tensile test |