Skip to main content
. 2018 Dec 10;9(12):653. doi: 10.3390/mi9120653

Table 5.

Optimization experiment investigating the effect of compression gap and holding pressure in the ICM of the COP material: (a) with two factors on two levels; (b) constant parameters.

(a) (b)
Factors Low Level High Level Parameters Value
Compression gap 0.4 mm 1.0 mm Injection velocity 40 mm/s
Holding pressure 250 bar 450 bar Switchover 10 mm
T melt COP 280 °C