Characteristic values for k, α, and ΔT = Tm − T0 and corresponding evaluation of TP for some metals of interest in laser-based powder bed fusion (L-PBF) [38,39].

Material k α ΔT = TmT0 TP = k/(α ×ΔT)
(W·m−1·K−1) (K1) (K) (W m−1 K−1)
AlSi10 [38] 113 22 × 10−6 570 ≈9000
Ti-6Al-4V [38] 6.7 9.2 × 10−6 1635 ≈445
Inconel 625 [39] 9.8 15 × 10−6 1330 ≈490
AISI316 [39] 16.2 16.2 × 10−6 1380 ≈725
Hastelloy X [39] 9.1 16 × 10−6 1335 ≈430
Cu [38] 391 17.7 × 10−6 1060 ≈21,000