Skip to main content
. 2018 Nov 29;11(12):2416. doi: 10.3390/ma11122416

Figure 1.

Figure 1

SEM images of drug loaded 24 wt.% 50:50 PLGA nanofibers (PLGA2).Images of same PLGA mat with different scale bars 100 µm (a), 50 µm (b), 10 µm (c) and 10 µm (d).