. 2018 Nov 28;11(12):2403. doi: 10.3390/ma11122403

Figure 4.

Figure 4

The thermal expansion curves (a) and transformed fraction curves (b) under 40 MPa tensile stress at a heating rate of 10, 15, 20 °C/min.