Parameters for masked DSCs using different additives and additive concentrations (see Table 3) in the electrolytes. Measurements were made on the day of sealing the cell. See Table S2 and Table S3 (Supporting Information File 1) for multiple cell data.

Electrolyte JSC [mA cm−2] VOC [mV] ff [%] η [%] Rel. η [%]

E1b 1.94 304 64 0.38 6.3
E2b 2.31 339 65 0.51 8.5
E3b 2.13 308 56 0.37 6.1
E4b 0.74 43 26 0.01 0.2
E2c 0.69 395 65 0.18 2.9
E2d 1.31 395 60 0.31 5.1
E2e 2.61 315 62 0.51 8.5
E2f 0.69 387 67 0.18 2.9
E2g 1.16 380 65 0.29 4.8
E2h 0.76 541 62 0.26 4.3
N719 13.87 705 62 6.02 100