Skip to main content
. 2015 May 20;1(1):24–43. doi: 10.3390/gels1010024

Figure 3.

Figure 3

Water uptake (% in weight) for CMC-NPs and CMC-DAP hydrogels in water and in 0.15 M NaCl solution at their maximum swelling degree.