Skip to main content
. 2018 Dec 7;19(12):3937. doi: 10.3390/ijms19123937

Table 2.

The Bis-GMA/TEGDMA/AgNP nanocomposite samples studied and their names: Ph (photopolymerization), RT (room temperature polymerization), T (thermal polymerization).

AgNP Concentration in Nanocomposite (ppm) Sample Name
Photopolymerization Room Temperature Polymerization Thermal Polymerization
0 Ph0 RT0 T0
25 Ph25 RT25 T25
50 Ph50 RT50 T50
100 Ph100 RT100 T100
150 Ph150 RT150 T150
250 Ph250 RT250 T250
500 - RT500 T500
1500 - RT1500 T1500
5000 - - T5000