Representative stress–strain curves at 80 mm/min strain rate showing the effect of the dianhydride structure and annealing time at Tann = TSH on the general mechanical performance of undamaged samples (a, left) and the effect of healing time at Tann = TSH of healed samples (b, right). Ttest = 23 ± 2 °C.