Skip to main content
. 2018 Oct 15;51(21):8333–8345. doi: 10.1021/acs.macromol.8b01396

Figure 3.

Figure 3

Effect of the healing time (tSH) at the TSH = Ttan δ MAX on the recovery of the individual mechanical parameters: Young modulus (E), stress at yield (σy), stress at break (σb), and strain at break (εb) for different dianhydride types. Ttest = 23 ± 2 °C. Both pristine and healed samples were subjected to the same thermal treatment at TSH for a given tSH.