Table 2.

Composition of the gellifying molar mixtures, as determined through the use of the (OH)AlTSPc species, employed as a probe for the synthesis of ZrO2, TiO2 and SiO2 translucent monolithic xerogels.

Sample Alkoxide/Volume (mL) n-PrOH (mL) acac (mL) DMF (mL) HCl 0.248 M (mL) (OH)AlTSPc (mL) [Macrocycle] * mol/L
ZrO2 Zr(OPrn)4/3.8 mL 1.2 0.42 0.083 0.2 4.04 × 10−4
blank-ZrO2 Zr(OPrn)4/3.8 mL 1.2 0.42 0.2
TiO2 Ti(OPrn)4/3.0 mL 1.0 0.2 0.3 0.2 4.04 × 10−4
blankTiO2 Ti(OPrn)4/3.0 mL 1.0 0.2 0.2
SiO2 Si(OEt)4 = TEOS 9.8 0.5 10 5.0 10−3−10−7
blank-SiO2 Si(OEt)4 = TEOS 9.8 10 5.0

* [Macrocycle] = Macrocycle Concentration.