Skip to main content
. 2018 Dec 26;12(1):73. doi: 10.3390/ma12010073

Figure 4.

Figure 4

Tomographic images of SLM-processed AlSi10Mg samples at volumetric energy density (ɛ) about, 61.9 J/mm3 (a), 76.2 J/mm3 (b), 88.1 J/mm3 (c), and DA values about, (d): −0.5 mm; (e): 0.5 mm; (f): 1 mm.